Abstract:Titanium dioxide content of Ilmenite concentration is generally 40%~50%, and total iron content is generally 30%~45%. Both will cause interference to the determination of other components during the analysis process of ilmenite concentration. A lot of hydrolysis of titanium can cause failure in analysis work. Samples are decomposed by using hydrofluoric acid-aqua regia-sulfuric. In 8% sulfuric acid and 10% hydrochloric acid medium, using ICP-AES national standard material as the standard curve, the contents of titanium, iron, vanadium in ilmenite fine flour can be rapidly determined. The method is simple, selective and accurate.